SoftenerNewbie
New Member
Runxin Up-flow regeneration valve: https://www.run-xin.com/upload/20190627/153734581337.pdf
Purolite C100E Resin: 2.5 cu-ft in 13x54 tank
According to resin datasheet, I need 0.25 - 0.5 gpm/cu-ft of Nacl/Brine injection. That means at 5 liters/min, the required brine (calculated at 8lb/cuft) will be injected in less than 7 mins (Brine and Slow Rinse in 21 mins). But according to data sheet Brine should be 20-40 mins. How come my brine time is coming up so short?
Should I get injector with even lower flow? Even at 3.5 liters/min, Brine injection will be 7-8 mins. I feel like I'm calculating something wrong?
Purolite C100E Resin: 2.5 cu-ft in 13x54 tank
According to resin datasheet, I need 0.25 - 0.5 gpm/cu-ft of Nacl/Brine injection. That means at 5 liters/min, the required brine (calculated at 8lb/cuft) will be injected in less than 7 mins (Brine and Slow Rinse in 21 mins). But according to data sheet Brine should be 20-40 mins. How come my brine time is coming up so short?
Should I get injector with even lower flow? Even at 3.5 liters/min, Brine injection will be 7-8 mins. I feel like I'm calculating something wrong?